Coating Mix for Iron Ladle

Mainly used on the working lining  of the ladle where local melting loss is serious. It is also widely used in the working lining of the melt running ladle, launder and various kilns.

Product specification

Technical Data

Item

Al2O3-MgO                    coating mix

Al2O3-C castable mix

Al2O3(%)≥

60

60

MgO(%)≥

6

/

SiC(%)≥

/

15

SiO2%

/

/

Bulk Densityg/3;

2.4

2.4

Cold Crushing Strength

(MPa) ≥

110℃×24h

18

20

1000℃×3h

/

/

1350℃×3h

40

30

Modulus of Rupture

(MPa)≥

110℃×24h

2

2

1350℃×3h

5

7

Application

Mainly used for some melted part of molten iron ladle and the edge of molten iron ladle